Elevated-Temperature Mechanical Properties of Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics
dc.contributor.author | Trice, Rodney W. | en_US |
dc.contributor.author | Halloran, John W. | en_US |
dc.date.accessioned | 2010-04-01T15:16:11Z | |
dc.date.available | 2010-04-01T15:16:11Z | |
dc.date.issued | 2000-02 | en_US |
dc.identifier.citation | Trice, Rodney W.; Halloran, John W. (2000). "Elevated-Temperature Mechanical Properties of Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics." Journal of the American Ceramic Society 83(2): 311-316. <http://hdl.handle.net/2027.42/65741> | en_US |
dc.identifier.issn | 0002-7820 | en_US |
dc.identifier.issn | 1551-2916 | en_US |
dc.identifier.uri | https://hdl.handle.net/2027.42/65741 | |
dc.format.extent | 2198543 bytes | |
dc.format.extent | 3110 bytes | |
dc.format.mimetype | application/pdf | |
dc.format.mimetype | text/plain | |
dc.publisher | American Ceramics Society | en_US |
dc.publisher | Blackwell Publishing Ltd | en_US |
dc.rights | 2004 The American Ceramics Society | en_US |
dc.subject.other | Mechanical Properties | en_US |
dc.subject.other | Silicon Nitride | en_US |
dc.subject.other | Boron Nitride | en_US |
dc.title | Elevated-Temperature Mechanical Properties of Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics | en_US |
dc.type | Article | en_US |
dc.rights.robots | IndexNoFollow | en_US |
dc.subject.hlbsecondlevel | Materials Science and Engineering | en_US |
dc.subject.hlbtoplevel | Engineering | en_US |
dc.description.peerreviewed | Peer Reviewed | en_US |
dc.contributor.affiliationum | Materials Science and Engineering Department, University of Michigan, Ann Arbor, Michigan 48109-2136 | en_US |
dc.description.bitstreamurl | http://deepblue.lib.umich.edu/bitstream/2027.42/65741/1/j.1151-2916.2000.tb01191.x.pdf | |
dc.identifier.doi | 10.1111/j.1151-2916.2000.tb01191.x | en_US |
dc.identifier.source | Journal of the American Ceramic Society | en_US |
dc.identifier.citedreference | S. Baskaran, S. D. Nunn, D. Popovic, and J. W. Halloran, “ Fibrous Monolithic Ceramics: I, Fabrication, Microstructure, and Indentation Behavior,” J. Am. Ceram. Soc., 76 [ 9 ] 2209 – 16 ( 1993 ). | en_US |
dc.identifier.citedreference | S. Baskaran, and J. W. Halloran, “ Fibrous Monolithic Ceramics: II, Flexural Strength and Fracture Behavior of the Silicon Carbide/Graphite System,” J. Am. Ceram. Soc., 76 [ 9 ] 2217 – 24 ( 1993 ). | en_US |
dc.identifier.citedreference | S. Baskaran, and J. W. Halloran, “ Fibrous Monolithic Ceramics: III, Mechanical Properties and Oxidation Behavior of the Silicon Carbide/Boron Nitride System,” J. Am. Ceram. Soc., 77 [ 5 ] 1249 – 55 ( 1994 ). | en_US |
dc.identifier.citedreference | S. Baskaran, S. D. Nunn, and J. W. Halloran, “ Fibrous Monolithic Ceramics: IV, Mechanical Properties and Oxidation Behavior of the Alumina/Nickel System,” J. Am. Ceram. Soc., 77 [ 5 ] 1256 – 62 ( 1994 ). | en_US |
dc.identifier.citedreference | G. Hilmas, A. Brady, U. Abdali, G. Zywicki, and J. Halloran, “ Fibrous Monoliths: Nonbrittle Fracture from Powder-Processed Ceramics,” Mater. Sci. Eng., A, 195, 263 – 68 ( 1995 ). | en_US |
dc.identifier.citedreference | W. J. Clegg, K. Kendall, N. McN. Alford, T. W. Button, and J. D. Birchall, “ A Simple Way to Make Tough Ceramics,” Nature (London), 357 [ October 4 ] 455 – 57 ( 1990 ). | en_US |
dc.identifier.citedreference | A. J. Phillipps, W. J. Clegg, and T. W. Clyne, “ Fracture Behavior of Ceramic Laminates in Bending-I. Modeling of Crack Propagation,” Acta Metall., 41 [ 3 ] 805 – 17 ( 1993 ). | en_US |
dc.identifier.citedreference | M.-Y. He, and J. W. Hutchinson, “ Crack Deflection at an Interface Between Dissimilar Elastic Materials,” Int. J. Solids Struct., 25 [ 9 ] 1053 – 67 ( 1989 ). | en_US |
dc.identifier.citedreference | D. Kovar, M. D. Thouless, and J. W. Halloran, “ Crack Deflection and Propagation in Layered Silicon Nitride/Boron Nitride Ceramics,” J. Am. Ceram. Soc., 81 [ 4 ] 1004 – 12 ( 1998 ). | en_US |
dc.identifier.citedreference | C. A. Folsom, F. W. Zok, and F. F. Lange, “ Flexural Properties of Brittle Multilayer Materials: I, Modeling,” J. Am. Ceram. Soc., 77 [ 3 ] 689 – 96 ( 1994 ). | en_US |
dc.identifier.citedreference | D. Kovar, B. H. King, R. W. Trice, and J. W. Halloran, “ Fibrous Monolithic Ceramics,” J. Am. Ceram. Soc., 80 [ 10 ] 2471 – 87 ( 1997 ). | en_US |
dc.identifier.citedreference | B. H. King, and J. W. Halloran, “ Fibrous Monolithic Ceramic Laminates I: Properties and Behavior of Unidirectional Laminates,” unpublished work. | en_US |
dc.identifier.citedreference | G. A. Brady, “ Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics ”; Master's Thesis. University of Michigan, Ann Arbor, MI, 1996. | en_US |
dc.identifier.citedreference | D. R. Clarke, and G. Thomas, “ Grain Boundary in a Hot-Pressed MgO Fluxed Silicon Nitride,” J. Am. Ceram. Soc., 60 [ 11 – 12 ] 491 – 95 ( 1977 ). | en_US |
dc.identifier.citedreference | L. K. V. Lou, T. E. Mitchell, and A. H. Heuer, “ Impurity Phases in Hot-Pressed Si 3 N 4,” J. Am. Ceram. Soc., 61 [ 9 – 10 ] 392 – 96 ( 1978 ). | en_US |
dc.identifier.citedreference | R. L. Tsai, and R. Raj, “ Creep Fracture in Ceramics Containing Small Amounts of a Liquid Phase,” Acta Metall., 30 1043 – 58 ( 1982 ). | en_US |
dc.identifier.citedreference | M. D. Thouless, “ A Review of Creep Rupture in Materials Containing an Amorphous Phase,” Res Mech., 22, 213 – 42 ( 1987 ). | en_US |
dc.identifier.citedreference | D. E. Wittmer, B. E. Rodely, V. A. Knapp, and S. P. Etherton, “ Comparison of Properties for Formulations Prepared from Two Silicon Nitride Powders,” Ceram. Eng. Sci. Proc., 17 [ 3 ] 363 – 70 ( 1996 ). | en_US |
dc.identifier.citedreference | A. W. Moore, “ Characterization of Pyrolytic Boron Nitride for Semiconductor Materials Processing,” J. Cryst. Growth, 106, 6 – 15 ( 1990 ). | en_US |
dc.identifier.citedreference | N. J. Archer, “ The Preparation and Properties of Pyrolitic Boron Nitride,” High Temp. Chem. Inorg. Ceram. Mater., Proc. Conf. 1976, 30, 167 – 80 ( 1977 ). | en_US |
dc.identifier.citedreference | R. W. Trice, and J. W. Halloran, “ Influence of Microstructure and Temperature on the Interfacial Fracture Energy of Silicon Nitride/Boron Nitride Fibrous Monolithic Ceramics,” J. Am. Ceram. Soc., 82 [ 9 ] 2502 – 508 ( 1999 ). | en_US |
dc.identifier.citedreference | G. E. Hilmas, G. A. Brady, and J. W. Halloran, “ SiC and Si 3 N 4 Fibrous Monoliths: Nonbrittle Fracture from Powder-Processed Ceramics Produced by Coextrusion ”; pp. 609 – 14 in Ceramic Transactions, Vol. 51, Fifth International Conference on Ceramic Processing Science and Technology. Edited by H. Hausner, G. L. Messing, and S.-I. Hirano American Ceramic Society, Westerville, OH, 1994. | en_US |
dc.identifier.citedreference | R. W. Trice, and J. W. Halloran, “ The Mode I Fracture Toughness of a Small-Grained Silicon Nitride: Orientation, Temperature, and Crack Length Effects,” J. Am. Ceram. Soc., 82 [ 10 ] 2633 – 40 ( 1999 ). | en_US |
dc.identifier.citedreference | 24 ASTM Standard C 373-72, American Society for Testing and Materials, West Conshohocken, PA, 1982. | en_US |
dc.identifier.citedreference | 25 MIL-STD-1942, “ Flexural Strength of High Performance Ceramics at Ambient Temperatures,” November 1990. | en_US |
dc.identifier.citedreference | T. Rouxel, J.-L. Besson, C. Gault, P. Goursat, M. Leigh, and S. Hampshire, “ Viscosity and Young's Modulus of an Oxynitride Glass,” J. Mater. Sci. Lett., 8, 1158 – 60 ( 1989 ). | en_US |
dc.identifier.citedreference | W. A. Cutler, F. W. Zok, F. F. Lange, and P. G. Charalambides, “ Delamination Resistance of Two Hybrid Ceramic-Composite Laminates,” J. Am. Ceram. Soc., 80 [ 12 ] 3029 – 37 ( 1997 ). | en_US |
dc.identifier.citedreference | J. A. Todd, and Z.-Y. Xu, “ The High Temperature Creep Deformation of Si 3 N 4 -6Y 2 O 3 -2Al 2 O 3,” J. Mater. Sci., 24, 4443 – 52 ( 1989 ). | en_US |
dc.owningcollname | Interdisciplinary and Peer-Reviewed |
Files in this item
Remediation of Harmful Language
The University of Michigan Library aims to describe library materials in a way that respects the people and communities who create, use, and are represented in our collections. Report harmful or offensive language in catalog records, finding aids, or elsewhere in our collections anonymously through our metadata feedback form. More information at Remediation of Harmful Language.
Accessibility
If you are unable to use this file in its current format, please select the Contact Us link and we can modify it to make it more accessible to you.